东莞市业强塑胶原料有限公司
POM , PC , PMMA , PA6 , PA66 , PC/ABS
PA66美国杜邦101L NC010

供应PA66塑胶原料 (1)PA66 美国液氮 R1000 HS,RA-1004,RAL-4022,RAL-4023,4026 ,4046,RB1008,RC1003,4536,RF10010HS,RF1007,RFL4026,RFL-4036 ,RL4010,RL-4040,PDX-R-02038,VF1002,AG6,25GF


 (2)PA66 美国首诺21SPC,21X-NC,22C,50BWFS,EC0315,M344 BK,M344-V0-BK,R513,R513H,R533,R533H,R543,R543H NC 

(3)PA66 美国杜邦:101F,101L,103FHS,103HSL,10B,10B40,11C40-BK,153HSL-NC010,3426,35L,408HS,409AHS-BK010,45SHB NC,5514,70G13HS1-L,70G13HS1L NC010,70G13L,70G13SH1L BK,70G20HSL,70G25HSL,70G25HSLR-BK099,70G30HSLR,70G33HSIL(BK),70G33HSIL(NC),70G33L,70G35HSL,70G35HSLC BK099,70G43L,70G43L-NC010,70G60L,72G13HS1L,72G33W NC010,73G30HSL,74G20HSL BK,74G33J,79G13HSL-NC,8018,8018HS,8061,80G14AHS-BK099,84G33,70G33HS1L-BK,80G33L-NC010,A73G15L BK083,AFE-9021-BK010,CFE8005HS BK,DMX65G30AH,EFE4068B BK,EFE7390 BK,FE130004-BK153J,FE13050,FE15004,FE15033,FE170007-BK031,FE5313 BK,FE5382,FE5514 NC010,FR15,FR50,FR52G20LX,FR52G30BL,FR52G30LX,FR52G35BL,FR52G45BL,FR53G50HSLR,FR7025,FR7025V0F NC010,FR7026V0F NC010,FR72G25V0 NC010,HTN 54G50HSL BK,HTN51G35HSL,HTN52G30NH,HTN52G45 BK,HTN53G35HSLR,HTN53G50HSLR,HTN53G50RHF,HTNFR52G30LX,ST801,ST-801,ST-801HS,ST801NC,ZYTA197

(4)PA66 日本旭化成1300G,1300G BK,1330G,1402S,14G25,14G33,1532S,54G43 NC,90G60,CR103,FR370-NC,TR161,WG143,54G33,1300S-BK,1300S,1402G-BK,90G55,CR301,FG172 BK,FG172X61,FG173X31,FR200,FR370,XN-T102,1300GT,93G33 X01 BK NC

 (5)PA66 日本三菱 N252D.3010N.3010GN15.3021GH-30

 (6)PA66 意大利兰蒂奇A45L1 (7)PA66 德国巴斯夫A3EG10,A3WG5 NC,A3WG5-BK,A3WG6,A3WG6-BK,A44,A4K,A3WG8(BK),A3X2G5 BK,A3Z,1403-2(GF13),8233G,1310-11,1403-2,8231GHS,A3EG10 NC,A3EG3,A3EG6,A3EG7,A3HG6,A3K,A3WG10,A3WG7,A3WU NC Q601,A3X2G5,A3X2G7,B40L,C4,C3U

注塑模工艺条件:干燥处理:如果加工前材料是密封的,那么就没有必要干燥。然而,如果储存容器被打开,那么建议在85℃的热空气中干燥处理。如果湿度大于0.2%,还需要进行105℃,12小时的真空干燥。熔化温度:260~290℃。对玻璃添加剂的产品为275~280℃。熔化温度应避免高于300℃。模具温度:建议80℃。模具温度将影响结晶度,而结晶度将影响产品的物理特性。对于薄壁塑件,如果使用低于40℃的模具温度,则塑件的结晶度将随着时间而变化,为了保持塑件的几何稳定性,需要进行退火处理。注射压力:通常在750~1250bar,取决于材料和产品设计 